Bearing steel pipe refers to hot rolled or cold rolled (cold drawn) seamless steel pipe used for manufacturing ordinary rolling bearing rings. The outer diameter of the steel pipe is 25-180mm, and the wall thickness is 3.5-20mm, which can be divided into two types: ordinary precision and higher precision.
Aanvraag sturen
Praat nu

Als toonaangevende leverancier en fabrikant in China levert GNEE Steel kosteneffectieve, op nikkel- gebaseerde legeringsproducten.

product Introductie

 

Bearing steel pipe refers to hot rolled or cold rolled (cold drawn) seamless steel pipe used for manufacturing ordinary rolling bearing rings. The outer diameter of the steel pipe is 25-180mm, and the wall thickness is 3.5-20mm, which can be divided into two types: ordinary precision and higher precision. Bearing steel is used to make balls, rollers and bearing rings. Bearing works under great pressure and friction, so bearing steel is required to have high and uniform hardness, wear resistance and high elastic limit.product-1-1

The requirements for the uniformity of chemical composition, the content and distribution of non-metallic inclusions, and the distribution of carbides of bearing steel are very strict. It is one of the most stringent steel grades in all steel production.

Relevant Steel Specification of 100Cr6 Bearing Steel

ASTM A295 DIN 17230 JIS G4805 BS 970
52100 100Cr6/1.3505 SUJ2 535A99/EN31

Chemical Composition of 100Cr6 Bearing Steel and Equivalents

C P S
ASTM A295 52100 0.93-1.05 0.25-0.45 0.025 0.015 0.15-0.35 0.25 1.35-1.60 0.30 0.10
DIN 17230 100Cr6/1.3505 0.90-1.05 0.25-0.45 0.030 0.025 0.15-0.35 0.30 1.35-1.65 0.30
JIS G4805 SUJ2 0.95-1.10 0.50 0.025 0.025 0.15-0.35 1.30-1.60
BS 970 535A99/EN31 0.95-1.10 0.40-0.70 0.10-0.35 1.20-1.60