Inconel is a versatile alloy, which is used in several industries. The Inconel 600 is a nickel-chromium alloy, which is highly resistant to corrosion. This alloy doesn't dissociate or deform easily under high pressures or elevated temperatures. Made up of superior strength the Inconel Alloy 600 has excellent mechanical properties. It has a minimum tensile strength of 760Mpa and a minimum yield strength of 585Mpa. These alloys can be easily elongated by 10% and still possess excellent workability. We are the leading Inconel 600 suppliers in the country. We supply high-quality products through all our outlets.
Controleren Inconel Legering 600 Materiaal Prijs per kg in China
The Inconel 600 melting point is in the range between 1354 to 1413 degrees C. This enables them to be used in heat treatment systems, chemical, food processing, phenol condensers, pressure vessels, etc. In the Inconel 600 thermal, conductivity is between 70 to 800 degrees F. They have this conductivity between 14.8 W/m·K to 20.9 W/m·K metric units. This helps in reducing running costs and operating material. The Inconel 600 machinability enables it to be drawn in square, rectangular, circular, and various other shapes. This alloy shows resistance against post-weld carburization and graining. The products of this grade are available in threaded, plain, and beveled ends. There are a few Inconel Alloy 600 equivalent grades. One of them is the UNS No6600 grade, which has similar strengths and mechanical properties as the 600 Inconel grade. These products are hardened as they are annealed after the hot-rolling process. Under the guidance of our workers, all our products are manufactured using the best raw materials and latest technology.


Inconel 600 Specificatie
Weergave Inconel 600 Equivalent, Smelten Punt, Thermisch Geleidbaarheid, Samenstelling, Bewerkbaarheid en Hardheid
| Normen | Inconel 600 |
|---|---|
| Verenigde Naties | N06600 |
| 2.4816 |
Inconel Alloy 600 Chemical Compostion
| Inconel 600 | |
| 72.{1} min | |
| Cr | 14.0 – 17.0 |
| 6.0 – 10.0 | |
| C | 0.15 max |
| Mn | 1.0 max |
| S | 0.015 max |
| Si | {0}.5 max |
| Cu | {0}.5 max |
Inconel legering 600 mechanisch sterkte
| Dichtheid | 8,47 g/cm3 |
| Smelten Punt | 1413 graad (2580 graad F) |
| Treksterkte sterkte | Psi–95,000, MPa – 655 |
| Opbrengst Sterkte (0.2%Offset) | Psi – 45,000 , MPa – 310 |
| Verlenging | 40 % |
Inconel 600 Toepassing
Inconel 600 gebruik in Thermokoppels
Inconel 600 gebruik in Nucleair Componenten
Inconel 600 gebruik in Papier & Pulp Industrie
Inconel 600 gebruik in Warmte Wisselaar
Inconel 600 gebruik in Chlorering Apparatuur
Inconel 600 gebruik in Petrochemie