Monel UNS N04400 metalen legeringflens
video

Monel UNS N04400 metalen legeringflens

Legering 400 flenzen in verschillende maten
Monel 400 grade flenzen: 1/2 in . (15 nb) tot 48 in . (1200nb)
Monel 400 blinde flenzen: 1/2 in . nb - 24 in . nb
Monel 400 UNS N04400 Slip-on flenzen: 1/2 in . nb-12 in . nb
Aanvraag sturen
Praat nu

Als toonaangevende leverancier en fabrikant in China levert GNEE Steel kosteneffectieve, op nikkel- gebaseerde legeringsproducten.

product Introductie

 

 

Monel 400 metalen legering flens beschrijving

What is the difference between nickel alloy C22 and Hastelloy C276

 

Kundige staalFlens van 400 metalen legering

Monel 400 flanges are made of a corrosion resistant, high strength nickel-copper super alloy. This material is easily weldable and has good formability. Gnee Steel is a large manufacturer and supplier of such flanges. These flanges are available in different pressure classes, from Class 150 Monel UNS N04400 flanges to Class 2500, from PN6 to Pn 64. De klasse definieert de drukcapaciteit . De samenstelling van Monel 400 Flenches omvat 63% nikkel en 28% koper, waardoor het sterker is . Alloem 400 BLANGEN GEBRUIKEN EEN SPECTEERDE PIPES MET ORIFICE PLATEN .}}} De materiaal heeft een minimum van 195MPA en een minimum. Tensiele sterkte van 480MPa . Er zijn verschillende normen om flenzen van verschillende nominale boorgroottes te dekken . ANSI B16 . 5 Monel DIN 2.4360 Blinde flenzen, die variëren van ½ inch tot 48 inch in diameter.

Afmetingen van UNS N04400 flens

Dimensions Of UNS N04400 Flange

Nominale maat Buitendiameter
(OD)
Min . dikte
(T)
Rf dia .
(R)
Geen . van boutgaten Diameter van gaten Boutcirkel
(BC)
Dus boor ID
(SB)
DIA . Hubbasis
(HB)
Dia . Hub Top
(HT)
Dus lth
(SL)
Wn lth
(WL)
* Wn boring -ID
(WB)
1⁄2 4.75 0.88 1.38 4 0.88 3.25 0.88 1.50 0.84 1.25 2.38 *
3⁄4 5.12 1.00 1.69 4 0.88 3.50 1.09 1.75 1.05 1.38 2.75 *
1 5.88 1.12 2.00 4 1.00 4.00 1.36 2.06 1.32 1.62 2.88 *
11⁄4 6.25 1.12 2.50 4 1.00 4.38 1.70 2.50 1.66 1.62 2.88 *
11⁄2 7.00 1.25 2.88 4 1.12 4.88 1.95 2.75 1.90 1.75 3.25 *
2 8.50 1.50 3.63 8 1.00 6.50 2.44 4.12 2.38 2.25 4.00 *
21⁄2 9.62 1.62 4.13 8 1.12 7.50 2.94 4.88 2.88 2.50 4.12 *
3 10.50 1.88 5.00 8 1.25 8.00 – 5.25 3.50 – 4.62 *
4 12.25 2.12 6.19 8 1.38 9.50 – 6.38 4.50 – 4.88 *
5 14.75 2.88 7.31 8 1.63 11.50 – 7.75 5.56 – 6.12 *
6 15.50 3.25 8.50 12 1.50 12.50 – 9.00 6.63 – 6.75 *
8 19.00 3.62 10.63 12 1.75 15.50 – 11.50 8.63 – 8.38 *
10 23.00 4.25 12.75 12 2.00 19.00 – 14.50 10.75 – 10.00 *
12 26.50 4.88 15.00 16 2.12 22.50 – 17.75 12.75 – 11.12 *
14 29.50 5.25 16.25 16 2.38 25.00 – 19.50 14.00 – 11.75 *
16 32.50 5.75 18.50 16 2.63 27.75 – 21.75 16.00 – 12.25 *
18 36.00 6.38 21.00 16 2.88 30.50 – 23.50 18.00 – 12.88 *
20 38.75 7.00 23.00 16 3.12 32.75 – 25.25 20.00 – 14.00 *
24 46.00 8.00 27.25 16 3.63 39.00 – 30.00 24.00 – 16.00 *

UNS N04400 metalen legeringsflensspecificatie

Chemische eigenschappen van Monel 400 UNS N04400 Pijpflens

Monel 400 Ni C Al Mn Si Fe Cu S Co Cr
63.0 min 0,3 Max 0,50 Max 2.0 Max 0,5 Max 1.0 – 2.5 28.0 – 34.0 0,02 Max – –

Legering 400 flens mechanische eigenschappen

Element Dikte Smeltpunt Treksterkte Opbrengststerkte (0,2%offset) Verlenging
ASTM B564 Monel 400 8,8 g/cm3 1350 graden (2460 graden F) Psi - 80, 000, MPA - 550 Psi - 35, 000, MPA - 240 40 %

Legering 400 flensdrukclassificatie

Temp ., graad Monel 400 flenzen werkdruk per klassen, bar
  150 300 400 600 900 1500 2500
-29 ~ 38 20.0 51.7 68.9 103.4 155.1 258.6 430.9
50 19.5 51.7 68.9 103.4 155.1 258.6 430.9
100 17.7 51.5 68.7 103.0 154.6 257.6 429.4
150 15.8 50.3 66.8 100.3 150.6 250.8 418.2
200 13.8 48.6 64.8 97.2 145.8 243.4 405.4
250 12.1 46.30 61.7 92.7 139.0 231.8 386.2
300 10.2 42.9 57.0 85.7 128.6 214.4 357.1
325 9.3 41.4 55.0 82.6 124.0 206.6 344.3
350 8.4 40.3 53.6 80.4 120.7 201.1 335.3
375 7.4 38.9 51.6 77.6 116.5 194.1 323.2
400 6.5 36.5 48.9 73.3 109.8 183.1 304.9
425 5.5 35.2 46.5 70.0 105.1 175.1 291.6
450 4.6 33.7 45.1 67.7 101.4 169.0 281.8
475 3.7 31.7 42.3 63.4 95.1 158.2 263.9
500 2.8 28.2 37.6 56.5 84.7 140.9 235.0
538 1.4 16.5 22.1 33.1 49.6 82.7 137.9
550 - 13.9 18.6 27.9 41.8 69.7 116.2
575 - 9.4 12.6 18.9 28.3 47.2 78.6
600 - 6.6 8.9 13.3 19.9 33.2 55.3
625 - 5.1 6.8 10.3 15.4 25.7 42.8
650 - 4.7 6.3 9.5 14.2 23.6 39.4

Monel 400 Ally Flens Application

UNS N04400 flensgebruik

ASTM B564 UNS N04400 flens worden gebruikt in toepassingen die uitstekende corrosieweerstand en hoge sterkte vereisen .

Ze worden gebruikt in chemische verwerkingsindustrieën voor de productie van zuren, alkalis en andere chemicaliën .

UNS N04400 Socket -lasflens wordt gebruikt in de maritieme industrie in scheepsbouw, offshore -platforms, ontziltingsinstallaties van zeewater, enz. .

Ze zijn te vinden in de olie- en gassector zoals offshore boorplatforms, pijpleidingen en onderzeese apparatuur .

UNS 4400 vervalste flens zijn te vinden in stroomopwekkingsfaciliteiten, waaronder energiecentrales en stoomturbinesystemen .

Ze worden ook gebruikt in de ruimtevaart- en farmaceutische industrie .

Uns n04400 legeringsflensverpakking

UNS N04400 Alloy Flange Packing
400 Alloy Flange Packing

Uns n04400 legeringsflensverpakking 

Over Gnee Steel

Gnee Steel

 

Over Gnee Steel

Gnee Steel is een leverancier van 400 metalen legeringflens, bedekkende buizen: naadloze buizen: maat: 4 - 219 mm; dikte: 0.5 - 20 mm; gelaste buizen: size: 5.0 - 1219.2 mm; dikte: 0.5 - 20 mm, platen: plaatdikte 0 . 1 tot 100 mm; Plaatbreedte 10-2500 mm, strips, legeringsronde staafgrootte: diameter 3-800 mm;, platte staafgrootte: dikte 2-100 mm; Width: 10-500 mm, zeshoekige balkgrootte: 2-100 mm;, draad en geëxtrudeerde profielen . We werken met staalfabrieken om klanten te voorzien van 625 legering, en overtreffen veel toonaangevende industrienormen, waaronder ASTM, ASME, AMS, AMS, ISO, ESO, DIN, EN en BS -normen.
GNEE stalen voorraden en verkoopt 400 metalen legeringflens, pijp, buis, plaat, strip, plaat, ronde balk, platte balk, smeden biljet, zeshoek, draad en extrusie . U bent van harte welkom om contact met ons op te nemen voor een offerte op elk gewenst moment bijss@gneesteel.com