8x4 gelegeerd 600 plaatgewicht, 600 stalen plaatafmetingen, Nee. 18 stalen plaatdikte, Inconel 600 metalen plaatdikte (mm), 600 gelegeerde metalen plaatafmetingen, Nee. 14 stalen plaatdikte, UNS N06600 stalen plaat maattabel.
inconel 600 plaat- en plaatgewichtgrafiek
| Plaatdikte (mm) | Gewicht (kg/m2) | kg/meter (breedte 1200 mm) | kg/meter (breedte 1500 mm) | kg/meter (breedte 1800 mm) | kg/meter (breedte 2400 mm) |
| 3 | 23.55 | 28.3 | 35.3 | 42.4 | 56.5 |
| 4 | 31.4 | 37.7 | 47.1 | 56.5 | 75.4 |
| 5 | 39.25 | 47.1 | 58.9 | 70.7 | 94.2 |
| 6 | 47.1 | 56.5 | 70.7 | 84.8 | 113 |
| 8 | 62.8 | 75.4 | 94.2 | 113 | 150.7 |
| 10 | 78.5 | 94 | 118 | 141 | 188 |
| 12 | 94.2 | 113 | 141 | 170 | 226 |
| 16 | 125.6 | 151 | 188 | 226 | 301 |
| 20 | 157 | 188 | 236 | 283 | 377 |
| 22 | 172.7 | 207 | 259 | 311 | 415 |
| 25 | 196.25 | 236 | 294 | 353 | 471 |
| 28 | 219.8 | 264 | 330 | 396 | 528 |
| 32 | 251.2 | 301 | 377 | 452 | 603 |
| 36 | 282.6 | 339 | 424 | 509 | 678 |
| 40 | 314 | 377 | 471 | 565 | 754 |
| 45 | 353.25 | 424 | 530 | 636 | 848 |
| 50 | 392.5 | 471 | 589 | 707 | 942 |
| 55 | 431.75 | 518 | 648 | 777 | 1036 |
| 60 | 471 | 565 | 707 | 848 | 1130 |
| 65 | 510 | 612 | 765 | 918 | 1224 |
| 70 | 549.5 | 659 | 824 | 989 | 1319 |
| 75 | 588.75 | 707 | 883 | 1060 | 1413 |
| 80 | 628 | 754 | 942 | 1130 | 1507 |
| 90 | 706.5 | 848 | 1060 | 1272 | 1696 |
| 100 | 785 | 942 | 1178 | 1413 | 1884 |
Uns N06600 Plaatdikte en gewicht – Engelse eenheden
| Nominale maat Dikte (inch) | Gewicht (lb/ft2) |
| 3/16 | 7.65 |
| 1/4 | 10.2 |
| 5/16 | 12.8 |
| 3/8 | 15.3 |
| 7/16 | 17.9 |
| 1/2 | 20.4 |
| 9/16 | 22.9 |
| 5/8 | 25.5 |
| 11/16 | 28.1 |
| 3/4 | 30.6 |
| 13/16 | 33.2 |
| 7/8 | 35.7 |
| 1 | 40.8 |
| 1 1/8 | 45.9 |
| 1 1/4 | 51.0 |
| 1 3/8 | 56.1 |
| 1 1/2 | 61.2 |
| 1 5/8 | 66.3 |
| 1 3/4 | 71.4 |
| 1 7/8 | 76.5 |
| 2 | 81.6 |
| 2 1/8 | 86.7 |
| 2 1/4 | 91.8 |
| 2 1/2 | 102 |
| 2 3/4 | 112 |
| 3 | 122 |
| 3 1/4 | 133 |
| 3 1/2 | 143 |
| 3 3/4 | 153 |
| 4 | 163 |
| 4 1/4 | 173 |
| 4 1/2 | 184 |
| 5 | 204 |
| 5 1/2 | 224 |
| 6 | 245 |
| 6 1/2 | 265 |
| 7 | 286 |
| 7 1/2 | 306 |
| 8 | 326 |
| 9 | 367 |
| 10 | 408 |
Legering 600 Plaatdikte en gewicht – metrische eenheden
| Plaatdikte (mm) | Gewicht (kg/m2) |
| 1.6 | 12.6 |
| 2.0 | 15.7 |
| 2.5 | 19.6 |
| 3 | 23.6 |
| 3.2 | 25.1 |
| 4 | 31.4 |
| 5 | 39.3 |
| 6 | 47.1 |
| 8 | 62.8 |
| 10 | 78.5 |
| 12.5 | 98.1 |
| 15 | 118 |
| 20 | 157 |
| 22.5 | 177 |
| 25 | 196 |
| 30 | 236 |
| 32 | 251 |
| 35 | 275 |
| 40 | 314 |
| 45 | 353 |
| 50 | 393 |
| 55 | 432 |
| 60 | 471 |
| 65 | 510 |
| 70 | 550 |
| 75 | 589 |
| 80 | 628 |
| 90 | 707 |
| 100 | 785 |
| 110 | 864 |
| 120 | 942 |
| 130 | 1051 |
| 150 | 1178 |
| 160 | 1256 |
| 180 | 1413 |
| 200 | 1570 |
| 250 | 1963 |